Customization: | Available |
---|---|
Carrier: | PP PE, PP, PE, PS, ABS, EVA |
Color: | All Colors, White |
Suppliers with verified business licenses
Using Method: Stir desiccant masterbatch and the damp plastic raw material uniformly, then produce product. For example, for blown film production, the addition ratio is 1%-2%. For sheet and injection molding production, the ratio is 2%-5%. For pipe production, add 2%-5%. The specific production should be added according to the moisture content of the plastic.
Note: 1. The masterbatch should be avoided mosture absorption before use.
2. It is best to use with ingredients immediately.
3. It should not be heated and dried with damp plastic to avoid poor quality during processing.
4. Check the packaging is whether intact or not before opening the package and seal packaging of unused masterbatch as soon as possible.
Technical parameter:
Carrier |
PE/PP |
Content of CaO |
75-80% |
Color |
White/ black/ grey |
Water absorption rate |
≥20% |
MFI21.6KG/190ºC |
5-40g /10mim |
Melting point |
140ºC-200ºC |
Phase fusibility |
PE/PP/PVC/ ABS |