Customization: | Available |
---|---|
Material: | Polyethylene/PE |
Usage: | General Plastics |
Still deciding? Get samples of US$ 95/kg
Request Sample
|
Suppliers with verified business licenses
No. | Property | Unit | Test | Data |
1 | Melt Flow Index | g/10min | GB/T3682-2000 | ≤2.0 |
2 | Density | g/cm3 | GB/T1033.1-2008 | ≤0.955-0.978 |
3 | Tensile strength | Mpa | GB/T1040.3-2006 | ≥20.0 |
4 | Tensile yield strength | Mpa | GB/T1040.3-2006 | ≥16 |
5 | Elongation at break | % | GB/T1040.3-2006 | ≥650 |
6 | Brittle temperature at low temperature | °C | GB/T5470-2008 | ≤-76 |
7 | ESCR ,FO | H | GB/T2951.41-2008 | ≥500 |
8 | Oxidation induction period at 200°C | Min | GB/T2951.42-2008 | ≥30 |
9 | Content of Carbon black | % | GB/T2951.41-2008 | 2.60±0.25 |
10 | Carbon Black dispersion | -- | GB/T18251-2000 | ≤3 |
11 | Ceka softening point | °C | GB/T1633-2000 | 110 |
12 | Tensile strength after thermal aging | Mpa | GB/T2951.12-2008 | ≥20.0 |
12 | Elongation after thermal aging | % | GB/T2951.12-2008 | ≥650 |
13 | Elongation at Low Temperature | % | GB/T2951.14-2008 | ≥175 |
16 | Dielectric strength | Mv/m | GB/T1408.1-2006 | ≥25 |
17 | Volume resistivity | Ω.m | GB/T1410-2006 | ≥1*1014 |
18 | Dielectric Constant ε | F/m | GB/T1409-2006 | ≤2.75 |
19 | Dielectric loss factor tgδ | -- | GB/T1409-2006 | ≤0.005 |