Customization: | Available |
---|---|
Material: | Polypropylene/PP |
Usage: | General Plastics |
Still deciding? Get samples of US$ 40/Bag
Request Sample
|
Suppliers with verified business licenses
Specifications |
|
Melt flow rate |
3.5 g/10 min (230°C/2.16kg) |
Density |
0.903 g/cm³ |
Tensile Stress at Yield |
30MPa |
Tensile Strain at Yield |
4 % |
Flexural modulus |
1300 (23 °C) |
Charpy notched impact strength |
9.0 kJ/m² (23 °C) |
Mold shrinkage |
1.3 |
Application: