Property | Unit | Test Method | Test Condition | HIPS |
Tensile Strength | kg/cm2 ( MPa) |
ASTM D-638 ( ISO527) |
23°C | 220 (22) |
Tensile Elongation | % | ASTM D-638 ( ISO527) |
23°C | 40 |
Flexural Strength | kg/cm2 ( MPa) |
ASTM D-790 ( ISO178) |
23°C | 440 (43) |
Flexural Modulus | kg/cm2*104 ( MPa) |
ASTM D-790 ( ISO178) |
23°C | 2.3 (2260) |
Izod Impact Strength |
kg-cm/cm ( J/m ) |
ASTM D-256 ( ISO R180 ) |
23°C 1/4'' bar |
11.0 (108) |
Vicat Softening Temperature |
°C | ASTM D-1525 (ISO306B) |
Annealed 80°C×2Hr 1/8'' bar |
95 |
Heat Deflection Temperature |
°C | ASTM D-648 ( 75/A) |
Annealed 80°C×2Hr 1/8'' bar |
88 |
Melt Flow Index |
g/10 min | ASTM D-1238 ( ISO1133 ) |
200°C×5Kg ( 49N ) |
5.5 |
Residual Monomer | ppm max. | - | - | 700 |
Molding Shrinkage |
% | FCFC Method |
23°C | 0.4~0.6 |
Specific Gravity | - | ASTM D-792 ( ISO1183 ) |
23°C/23°C | 1.04 |
Flammability | - | UL-94 | FILE NO. E162823 |
1/16" HB NC |
Raw materials description | |||||||
Standard | Injection molding grade | Colour | White | ||||
Application | High impact, high heat-resisting, low temperature resistance,good regidity,according with food hygienic standard, be widely used in toy and home appliances manufacture. | ||||||
Remark | High impact, high heat-resisting, extrusion molding. | ||||||
Raw materials technique data | |||||||
Property items | Test condition | Method | Test result | Units | |||
Basic performance | Melt flow rate | 200°C/5kg | ISO 1133 | 4.6 | g/10min | ||
Density | ISO 1183 | 1.04 | g/cm3 | ||||
Water absorption | ISO 62 | <0.1 | % | ||||
Physical property | Process contractibility rate | ISO 294 | 0.4-0.7 | % | |||
Mechanical behavior | Stretch yield stress | 23°C | ISO 527 | 23 | Mpa | ||
Percentage elongation | 23°C | ISO 527 | 45 | % | |||
flexural strengh | 23°C | ISO 178 | 46 | Mpa | |||
Flexural modulus | 23°C | ISO 178 | 2260 | Mpa | |||
Izod impact | 23°C | ISO 180 | 115 | j/m | |||
Rockwell hardness | 23°C | ASTMD-785 | 65 | L | |||
Thermal property |
Vicat softening point | B10/oil | ISO 306 | 95 | °C | ||
distortion temperature(non-anneal) | 1.82Mpa | ISO 75-2 | 79 | °C | |||
Other propery | Fire resistance | UL 94 | HB | ||||
residual monomer | <400 | ppm max | |||||